Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 160 - 180 °C | 320 - 356 °F | |
Sibur 1045-12 Compound 948 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Softening Point | 160 - 180 °C | 320 - 356 °F | |
Sibur O-40 Compound 239 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Softening Point | 160 - 180 °C | 320 - 356 °F | |
Sibur O-40 Compound OM-40 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Softening Point | 160 - 180 °C | 320 - 356 °F | |
Sibur O-55 Compound 1182 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |