Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 108 - 128 °C | 226 - 262 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-583 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 108 - 128 °C | 226 - 262 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-592 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 108 - 128 °C | 226 - 262 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-782 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized... |