Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 70.0 - 80.0 °C | 158 - 176 °F | Average value: 76.8 °C Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Softening Point | 70.0 - 80.0 °C | 158 - 176 °F | MQSA 70A |
Lubrizol Advanced Materials Pearlbond® Eco D900 Thermoplastic Polyurethane Pearlbond™ ECO D900 is a linear, aromatic polyurethane based on specialty polyol from renewable sources. It contains 67% of renewable material as certified according to ASTM-D6866. It is suppli.. |
|||
Softening Point | 77.0 - 80.0 °C | 171 - 176 °F | |
DayGlo Gem-Tone GC-18F Emerald Green Gem-Tone® GC-18F Emerald Green is a rich, strong green colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of .. |
|||
Softening Point | 70.0 - 80.0 °C | 158 - 176 °F | Kofler; MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® 118 Thermoplastic Polyurethane The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo.. |