Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 1275 °C | 2327 °F | Dilatometric @ 10psi |
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Softening Point | 1275 °C | 2327 °F | Dilatometric @ 10psi |
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |