Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 98.89 °C | 210.0 °F | ASTM D648 |
Lucent Polymers PC/ABS-1211P Polycarbonate+ABS, Impact Modified, Platable, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.89 °C | 210.0 °F | ASTM D648 |
Lucent Polymers PC/PBT-1212 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 98.89 °C | 210.0 °F | ASTM D648 |
Lucent Polymers PC/PBT-1422 Polycarbonate+PBT, Improved Cold Temp Impact, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |