Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C @Thickness 6.35 mm |
192 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne LubriOne™ AT-000/05T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | 0.125 in bar, Unannealed/Conditioned 48 hours; ASTM D648 |
Network Polymers NPP 808 C4WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers SAN 277 Blue Tint Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers SAN 278 Medium Blue Tint Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers SAN 279 Water White Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | ASTM D648 |
Kostat ICP-STAT ICS-1005 ABS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | ASTM D648 |
Kostat ICP-STAT ICD-1005 ABS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | Unannealed; ASTM D648 |
Entec Hyrene® PSCRY 1.5 General Purpose Polystyrene Available in North America Features: Crystal, High Heat Resistance, General Purpose, High Molecular WeightRoHS Compliant Form: Pellets Information provided by Entec |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS/PC 8901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics STYRON® 685D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsFoamOPSMedicalInformation provided by AmericasSty.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics STYRON® 685DL High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantTypical ApplicationsFoamOPSMedicalInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics STYRON® 665 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeFood Contact CompliantTypical ApplicationsFilmInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 88.9 °C | 192 °F | ASTM D648 |
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC. |