Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 84.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 84.0 °C
122 - 183 °F
Average value: 69.8 °C Grade Count:20
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Deflection Temperature at 1.8 MPa (264 psi) 44.0 - 84.0 °C
111 - 183 °F
Average value: 64.6 °C Grade Count:3
Overview of materials for ABS/Polyurethane Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr..