Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C

@Thickness 6.35 mm
181 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C

@Thickness 6.35 mm
181 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne LubriOne™ AT-000/20T Black Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
0.125 inch bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Network Polymers SBN 150 Styrene Butadiene Acrylonitrile Terpolymer
Description: Styrene Butadiene Acrylonitrile TerpolymerInformation provided by Network Polymers Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Unannealed; ASTM D648
M. Holland Company GS410WC Polystyrene  (discontinued **)
Features: High Clarity, High FlowUses: Household Goods, LabwareApprovals: FDA 21 CFR 177.1640 Processing Method: Injection MoldingInformation provided by M. Holland.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® ABS 8015 CL
Availability: North AmericaForms: PelletsFeatures: CopolymerAppearance: Clear/TransparentInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C

@Thickness 3.20 mm
181 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines..
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Unannealed; ASTM Data
Styron Magnumâ„¢ 344CC ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Unannealed; ASTM D648
Styron XU 73120.00 Polycarbonate Resin
Overview: XU 73120.00 Experimental Polycarbonate Resin is a high flow ignition resistant PC blend that contains no chlorinated or brominated additives. This resin is specifically designed to offer e..
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Unannealed; ASTM Data
Styron Magnumâ„¢ 344HP ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Diamond Polymers ABS 3003MC Black 1722
Description: BlackInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Diamond Polymers ABS 3500
Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
0.125 in bar Annealed 4 hours at 80°C; ASTM D648
Diamond Polymers ABS VP-12
Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Diamond Polymers ASA S150
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Diamond Polymers ASA S510
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
0.125 in bar Annealed 4 hours at 80°C; ASTM D648
Diamond Polymers TR 5000 AS/P
Description: Transparent ABS, Antistatic GradeInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
ASTM D648
Americas Styrenics STYRON® 404 High Impact Polystyrene
Product CharacteristicsAdditive FreeTypical ApplicationsCompounding and masterbatchesInformation provided by AmericasStyrenics LLC.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Aclo Accutech Polypropylene Copolymer HP0335W40L Wollastonite Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Aclo Accutech Polypropylene Homopolymer HP0339M40CL Mica Reinforced Coupled
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
ASTM D648
Americas Styrenics STYRON® 498 High Impact Polystyrene
Product CharacteristicsHigh glossHigh impactFood Contact CompliantUL Classification 94HBTypical ApplicationsAppliancesMedicalHousewaresConsumer electronicsInformation provided by AmericasStyrenics L..
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Unannealed (0.250"); ASTM D648
LTL Color Compounds ColorFast® GPA300 ABS
Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Unannealed (0.250"); ASTM D648
LTL Color Compounds ColorFast® GPA300X ABS
Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
Aclo Accucomp ABS ABS801V Automotive Approved Grade
Copyright © lookpolymers.com All Rights Reserved