Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 79.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 26.1 °C
79.0 °F
ASTM D648
Americas Styrenics STYRON® 484 High Impact Polystyrene
Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliances/RefrigerationPackaging/disposablesHousewaresInformation pr..