Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 75.5 °C | 168 °F | annealed; ASTM D648 |
Kleerdex Kydex® L Acrylic/PVC Thermoplastic Sheet
(discontinued **) Laminating grade fire rated sheetApplications: Store fixtures and displays, exhibits, service counters, doors, partitionsFeatures: Toughness and durability, solid, integral color, chemical resistanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.5 °C | 168 °F | annealed; ASTM D648 |
KYDEX® 311 Co-Extruded High Impact Fire-Rated Thermoplastic Sheet Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.5 °C | 168 °F | annealed; ASTM D648 |
KYDEX® 311 MB Co-Extruded High Impact Fire-Rated Thermoplastic Sheet with Microban® Antimicrobial Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.5 °C | 168 °F | annealed; ASTM D648 |
KYDEX® T Acrylic/PVC Thermoplastic Sheet Impact resistant fire rated sheetApplications: External housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for equipment such as v.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.5 °C | 168 °F | annealed; ASTM D648 |
KYDEX® 331/331d Co-Extruded High Impact Fire Rated Thermoplastic Sheet with Weatherable Acrylic Film Cap KYDEX® 331 is a co-extruded high impact fire rated thermoplastic sheet with a weatherable cap that offers superior performance for thermoforming. It can also be used as an impact resistant surfa.. |