Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C @Thickness 3.18 mm |
152 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 161JA White Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C @Thickness 1.57 mm |
152 °F @Thickness 0.0618 in |
Annealed; ASTM D648 |
PolyOne Novablend™ 2677 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | ISO 75-1 |
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | ASTM D648 |
RheTech Products RCT120-01 20% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC and I/P ComponentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | ASTM D648 |
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | ASTM D648 |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | unannealed; ASTM D648 |
KYDEX® 311 Co-Extruded High Impact Fire-Rated Thermoplastic Sheet Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | unannealed; ASTM D648 |
KYDEX® 311 MB Co-Extruded High Impact Fire-Rated Thermoplastic Sheet with Microban® Antimicrobial Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | unannealed; ASTM D648 |
KYDEX® 331/331d Co-Extruded High Impact Fire Rated Thermoplastic Sheet with Weatherable Acrylic Film Cap KYDEX® 331 is a co-extruded high impact fire rated thermoplastic sheet with a weatherable cap that offers superior performance for thermoforming. It can also be used as an impact resistant surfa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 FR IM BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: BlackTPCI# 9993101Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | ASTM D-648 |
Axiall 3020 Rigid PVC, Extrusion Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | ASTM D-648 |
Axiall 3217 Rigid PVC, Extrusion Georgia Gulf 3217 is a powder blend designed for the extrusion of window, door, fence and marine profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | annealed; ASTM D-648 |
Axiall 8150 Rigid PVC, Extrusion & Molding Georgia Gulf 8150 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | annealed; ASTM D-648 |
Axiall 3650 Rigid PVC, Extrusion Georgia Gulf 3650 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resistan.. |