Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C @Thickness 3.18 mm |
144 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-TB is a clear blue tint pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | ASTM D648 |
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | ASTM D648 |
Nylene® 9110 Unfilled Nylon 6/10 Description: Nylene® 9110 is an unfilled specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat Stabilized and High FlowRoHS CompliantAuto Specifications: GM GMP.PA66.074.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CMN 303 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for high heat ageing resistance for automotive interior trim applications such as instrument panels.Availability: Africa & Mi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | ASTM D648B |
ExxonMobil HDPE HD 6719.62 High Density Polyethylene Copolymer Resin Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Copolymer CP0436W30L1 Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0336C30L Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0336C40L Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0336C40L1 Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339C30L Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339C40L1 Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | ASTM D-648 |
Axiall 8302 Rigid PVC, Extrusion & Molding Georgia Gulf 8302 is a clear rigid PVC pellet compound suited for applications where transparency is important in a high sunlight environment. It can be used for exterior transparent profiles such .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339M10L Mica Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339T20L Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339T30L Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-20FG-0754 20% Glass, Heat Stabilized Information provided by Asahi Thermofil |