Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | Unannealed; ASTM D648 |
Multibase Nylex™ 2185 FR V0 Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
RheTech Products P256-762 Polypropylene Copolymer, Medium Grey Applications: Misc. ClipsElectrical housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
Nylene® 8100 Unfilled Nylon 6/12 Description: Nylene® 8100 is an unfilled specialty fiber. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ASTM D648 |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 - 138 °C | 127 - 280 °F | Average value: 86.8 °C Grade Count:9 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ CB259 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB259 medium high melt flow, 1,600 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hifaxâ„¢ DR279 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ DR279 high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a unique balance of stiffness, impact resistance, processability.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hostacomâ„¢ CB189FC/1 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB189FC/1 medium melt flow, 1,300 MPa flexural modulus, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact, stiffne.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CMU 101 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior trim in which good surface finish, high scratch resistance and good UV resistance are required.Availa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CMU 101D Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior trim in which good surface finish, high scratch resistance, minimum dust deposit and good UV resistan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | ISO 75-2/A |
ExxonMobil PP4031E2 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | |
Aclo Accutech Polypropylene Copolymer CP0436W10L1 Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | |
Aclo Accutech Polypropylene Copolymer CP0437T20L Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | |
Aclo Accutech Polypropylene Copolymer CP0437W20L1 Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | |
Aclo Accucomp Polypropylene HPO306L Homopolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | |
Aclo Accucomp Polypropylene HPO309L Homopolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 52.8 °C | 127 °F | |
Aclo Accutech Polypropylene Copolymer CP0436T10L1 Talc Reinforced |