Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ASTM D648
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ASTM D648
RheTech Products FT4700-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ASTM D648
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ASTM D648
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ASTM D648
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ASTM D648
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ASTM D648
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
Unannealed; ISO 75A-1, -2
LyondellBasell Moplen HP400L Polypropylene Homopolymer
Description: All ingredients in HP400L meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Toys, containers, lids, medical applications, closure capsInformation provid..
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
Unannealed; ISO 75A-1, -2
LyondellBasell Moplen HP400N Polypropylene Homopolymer
Description: HP400N is a high flow homopolymer with a conventional molecular weight distribution and is formulated with a general-purpose additive package. HP400N is designed for injection molding a..
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
Unannealed; ISO 75A-1, -2
LyondellBasell Moplen HP550J Polypropylene Homopolymer
Description: HP550J, a general purpose polypropylene homopolymer resin, is suitable for general extrusion and film fiber applications. HP550J resin meets FDA requirements in the Code of Federal Reg..
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
Unannealed; ISO 75A-1, -2
LyondellBasell Hostacomâ„¢ CB267 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB267 medium melt flow, 1,600 MPa flexural modulus thermoplastic elastomeric olefin (TEO) resin has an excellent balance of scratch and mar resistance, rigidity and impac..
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ISO 75-2/A
ExxonMobil Exxtral™ BNU 011 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for injection molded automotive interior applications.Availability: A..
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ISO 75-2/A
ExxonMobil PP7054L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with medium flow. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications..
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
Aclo Accutech Polypropylene Copolymer CP0436W10L Wollastonite Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
Aclo Accutech Polypropylene Copolymer CP0437C40L1 Calcium Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
Aclo Accutech Polypropylene Copolymer CP0437M10CL Mica Reinforced Coupled
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
Aclo Accutech Polypropylene Copolymer CP0437W10L1 Wollastonite Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ASTM D648
Cast Nylons Nycast® 12 Cast Nylon 12
NYCAST® 12 is specially formulated and designed to offer very low moisture absorption, superior wear resistance, dimensional stability, exceptional lubrication ability, outstanding mechanical chara..
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ISO 75-2/A
ExxonMobil Exxtral™ CNW 010 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior trim applications requiring low warpage.Availability: Africa & Middle East, Asia Pac..
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
ISO 75-2/A
ExxonMobil PP1364E2 Polypropylene Homopolymer
Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc..
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C

@Thickness 3.17 mm
124 °F

@Thickness 0.125 in
Unannealed; ISO 75-2-92
Styron INSPIRE™ TF3800 Polypropylene
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °C
124 °F
Unannealed; ISO 75A-1, -2
LyondellBasell Hifax™ ETA3163/1 Thermoplastic Polyolefin Elastomer
Description: Hifax™ ETA3163/1 medium melt flow, 900 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of stiffness and low temper..