Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
Unannealed; ASTM D648
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS
LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK
LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear
LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS (Asia Pacific)
LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber.This product is also known as Thermocomp* OF-1008.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP OF008AH PPS - Branched
LNP* THERMOCOMP* OF008AH is a compound based on PPS - Branched resin containing 40% Glass Fiber. Added features of this grade are: Healthcare.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp OF008E PPS
LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the A..
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - LINEAR
LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing 40% Glass Fiber. Added features of this material include: Easy Molding.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS (Asia Pacific)
LNP* Thermocomp* OF008E is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. Added features of this material include: Easy Molding.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66
LNP* THERMOCOMP* RC006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66
LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK (Asia Pacific)
LNP* Thermocomp* LF008 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched
LNP* THERMOCOMP* OF008A is a compound based on PPS - Branched resin containing 40% Glass Fiber.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66 (Asia Pacific)
LNP* Thermocomp* RC006 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP RC006H PA 66
LNP THERMOCOMP* RC006H is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific)
LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP VERTON RV008S PA 66
LNP* VERTON* RV008S is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C

@Thickness 3.20 mm
502 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP VERTON RV008S PA 66 (Asia Pacific)
LNP* Verton* RV008S is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP VERTON RX03013 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX03013 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
ASTM D648
Plenco 1530 Polyester, Briquette, Injection Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP VERTON RVL36SXS PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RVL36SXS is a compound based on PA 66 resin containing Long Glass Fiber, PTFE. Added features include; Internally Lubricated.
Deflection Temperature at 1.8 MPa (264 psi) 261 °C
502 °F
ASTM D648
Plenco 7552 Phenolic, Nodular, Injection Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..