Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black
Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
RheTech Products P250-00 Polypropylene Copolymer, Natural
Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural
Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black
Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
RheTech Products P251-00 Polypropylene Copolymer, Natural
Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
RheTech Products P254-00 Polypropylene Copolymer, Natural
Applications: Air ducts - distributionInterior trimI/P componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
RheTech Products P256-00 Polypropylene Copolymer, Natural
Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fender linersSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ASTM D648
Ineos N01G-02 Polypropylene Impact Copolymer
N01G-02 is a low melt flow rate polypropylene impact copolymer designed for blow molding, extrusion, and compounding applications. The grade benefits from a very high impact resistance at room and l..
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
ISO 75-2/A
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer
Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol..
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
BCC Products BC 7009-2 Epoxy Casting
BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in m..