Deflection Temperature at 1.8 MPa (264 psi) 253 °C
488 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear..
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
488 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) Features: Lubricated, Good Wear Resistance and Low Friction Appearance..
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
488 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta..