Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 465 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Oxford Polymers Oxtron PPS-XT-40GF PPS, 40% Glass Reinforced
Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy. Processing and Delivery Form: Pellets and Injection MoldingAppearance: Natural off-whit..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
ASTM D648
Polymer Resources NY66-G13 Nylon 66, 13% Glass Reinforced
Nylon 66, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N1233HL BK Nylon 6/6
Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantAuto Specifications: ..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
ASTM D648
Polymer Resources NY66-G13-[color]-H Nylon 66, 13% Glass Reinforced, Heat Stabilized
Nylon 66, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
ASTM D648
Polymer Resources NY66-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/6 CF10 TS15 BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(13%) and Silicone Lubricant(2%)Features: Lubricated Appearance: BlackInforma..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/6 GF30 TS1 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/6 GF30 TS15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® PA6/6,6 GF50 HS L 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® PA6/6,6 GF60 HS L 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302..
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Chase Plastics CP Pryme® NN313L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated, Recycled Content
Features: LubricatedRecycled ContentForm: PelletsInformation provided by Chase Plastics.
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® PA6/6 GF25 FR 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightUL File Number: E157318TPCI# 9085101Information provided by TP Composites, Inc.