Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C @Thickness 3.20 mm |
448 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | ASTM D648 |
Plenco 1508 Polyester, Briquette, Transfer Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | ASTM Test |
BASF Ultramid® 1403-2 BK ND3007 PA66 (Dry) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | ASTM Test |
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry) Ultramid 1403-2 NF3001 is a 13% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 630 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 231 °C | 448 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East) LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |