Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | ASTM D648 |
Nylene® Vexel™ B12GF15 SA , 15% Glass Reinforced PBT Description: Vexel™ B12GF15 SA is a 15% glass fiber reinforced PBT with improved surface aPolyphenylene Etherarance. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | ASTM D648 |
Nylene® Vexel™ B12GF30 FR , 30% Glass Reinforced, Flame Retardant PBT Description: Vexel™ B12GF30 FR is a 30% glass fiber reinforced, flame retardant PBT. B12GF30 FR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | 0.125 in bar; ASTM D648 |
Network Polymers Nylon 6G20L Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | ASTM D648 |
Oxford Polymers 15GF 15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) 15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT)Information provided by Oxford Polymers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GB20 L 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF/B20 A2 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformation .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PBT GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6 GF20 RM L BK Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Low Moisture Absorption and LubricatedBlackTPCI# 9718102Inf.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6 GF20 RM-B L NAT Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Low Moisture Absorption and LubricatedAppearance: BlackTPCI.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | ASTM D648 |
Chase Plastics CP Pryme® N110GL (COND, 50% RH) Nylon 6, 10% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | ASTM D648 |
Chase Plastics CP Pryme® N110GL (DAM) Nylon 6, 10% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | ASTM D648 |
Chase Plastics CP Pryme® N313GL (DAM) Nylon 6 (Utility Grade), 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | ASTM D648 |
Chase Plastics CP Pryme® N213GL (COND, 50% RH) Nylon 6, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | ASTM D648 |
Chase Plastics CP Pryme® N213GL (DAM) Nylon 6, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 191 °C | 375 °F | ASTM D648 |
Chase Plastics CP Pryme® N310GL (DAM) Nylon 6 (Utility Grade), 10% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |