Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 4012 X Platinum Polypropylene Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Polymer Resources PC-G20-[color]-1 Polycarbonate, 20% Glass Reinforced with Mold Release Polycarbonate, 20% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Polymer Resources PC-G20-[color]-WS Polycarbonate, 20% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PC 04009 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PC SS10 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: ConductiveInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PC SS15 FR BK 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® TPX-PC-02071 Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | unannealed; ASTM D648 |
Styron EMERGEâ„¢ 4731-8 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | unannealed; ASTM D648 |
Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® PC130R Polycarbonate, 30% Glass Fiber Reinforced Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | |
BCC Products HPX-850 Epoxy Backfill System HPX-850 is a light weight, heat resistant, two component epoxy backfill system. HPX-850 features advantages such as low cost, long pot life, machineability, and low shrinkage. HPX-850 is ideally su.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Polymer Resources PCSF-FRG20 Polycarbonate, 20% Glass Reinforced Structural Foam Grade Polycarbonate, 20% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 141 °C | 285 °F | ASTM D648 |
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |