Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.7 - 130 °C
170 - 266 °F
Average value: 98.1 °C Grade Count:122
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Deflection Temperature at 1.8 MPa (264 psi) 110 - 130 °C
230 - 266 °F
ISO 75-A
Raschig Group 3572 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis..
Deflection Temperature at 1.8 MPa (264 psi) 39.0 - 130 °C
102 - 266 °F
Average value: 92.7 °C Grade Count:13
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Deflection Temperature at 1.8 MPa (264 psi) 55.0 - 130 °C
131 - 266 °F
Average value: 81.1 °C Grade Count:24
Overview of materials for Polypropylene with 30% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are..