Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
ASTM D648
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
Annealed; ASTM D648
M. Holland Company PC522R Polycarbonate
High flowHigh impact resistanceGood mold releaseApplications: AppliancesFood containersTable products
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
Unannealed, 0.125 in; ASTM D648
Styron CALIBREâ„¢ 201-22 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
unannealed; ASTM D648
Styron CALIBREâ„¢ 2061-22 Polycarbonate
CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
0.157 in, unannealed; ASTM D648
Styron EMERGEâ„¢ 4310-22 Polycarbonate
EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
0.157 in, unannealed; ASTM D648
Styron EMERGEâ„¢ 4330-22 Polycarbonate
EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
Unannealed, 0.125 in; ASTM D648
Styron CALIBREâ„¢ 301 EP Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
Unannealed, 0.125 in; ASTM D648
Styron CALIBREâ„¢ 303 EP Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
Unannealed; ASTM D648
Chase Plastics CP Pryme® AH300 Acetal Homopolymer, Recycled Content
Features: General purposeHigh heat resistanceGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantHigh rigiditySolvent r..
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
258 °F
ASTM D648
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey
Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.