Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 106 °C
158 - 223 °F
Average value: 89.0 °C Grade Count:82
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Deflection Temperature at 1.8 MPa (264 psi) 92.2 - 106 °C
198 - 223 °F
Average value: 98.1 °C Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Deflection Temperature at 1.8 MPa (264 psi) 51.7 - 106 °C
125 - 223 °F
Average value: 89.2 °C Grade Count:211
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Deflection Temperature at 1.8 MPa (264 psi) 40.6 - 106 °C
105 - 223 °F
Average value: 59.7 °C Grade Count:56
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..