Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 189 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
ASTM D648
RedEye On Demand Polyphenylsulfone (PPSF), Rapid Prototyping Material
Polyphenylsulfone (PPSF) is a durable high-end thermoplastic that can be used in the toughest applications. Parts built in PPSF can handle heat near 400°F (204°C), it resists petroleum products, a..
Deflection Temperature at 1.8 MPa (264 psi) 189 - 221 °C
372 - 430 °F
Average value: 206 °C Grade Count:16
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea..
Deflection Temperature at 1.8 MPa (264 psi) 189 °C

@Thickness 3.18 mm
372 °F

@Thickness 0.125 in
Unannealed; ASTM D648
LNP ULTEM® SMU6303 Polyetherimide, 5% Glass Fiber Reinforcement, 5% PTFE Lubricant  (discontinued **)
Will be UNTW05.Features: Lubricated, High Heat Resistance, Good Wear Resistance, Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provide..
Deflection Temperature at 1.8 MPa (264 psi) 189 °C

@Thickness 3.20 mm
372 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA 6/12 (Asia Pacific)
LNP* LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C

@Thickness 3.20 mm
372 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66
LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics Ultem 2212 PEI (Europe-Africa-Middle East)
20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics ULTEM 2212R PEI (Europe-Africa-Middle East)
20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C

@Thickness 6.40 mm
372 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer
High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C

@Thickness 6.40 mm
372 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East)
High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
ASTM D648
Stratasys® Polyphenylsulfone
PPSF/PPSU (polyphenylsulfone) material has the greatest strength, heat and chemical resistance of all Stratasys materials - ideal for aerospace, automotive and medical applications. Stratasys FDM (F..
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI
LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C

@Thickness 3.20 mm
372 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI
LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI
LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10
LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C

@Thickness 6.40 mm
372 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific)
High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
ASTM D648
Plenco 4548 Phenolic, Granular, Transfer Molded
PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai..
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
ASTM D648
Clariant Renol 612G20-L Nylon 612, 20% Glass Fiber Reinforced, Lubricated
Data provided by Clariant Masterbatches
Deflection Temperature at 1.8 MPa (264 psi) 189 °C

@Thickness 3.20 mm
372 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON OE002 PPS - LINEAR
LNP* STAT-KON* OE002 is a compound based on PPS - Linear resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
ASTM D648
Proto3000 PPSF Fused Deposition Modeling Polymer
Description: PPSF/PPSU (polyphenylsulfone) material has the greatest heat and chemical resistance of all Fortus materials - ideal for aerospace, automotive and medical applications. PPSF parts manuf..
Copyright © lookpolymers.com All Rights Reserved