Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 89.0 - 177 °C
192 - 350 °F
Average value: 149 °C Grade Count:38
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Deflection Temperature at 1.8 MPa (264 psi) 175 - 177 °C
347 - 350 °F
Average value: 176 °C Grade Count:3
Overview of materials for Nylon 11 with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ..
Deflection Temperature at 1.8 MPa (264 psi) 154 - 177 °C
310 - 351 °F
Average value: 166 °C Grade Count:13
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Deflection Temperature at 1.8 MPa (264 psi) 130 - 177 °C
266 - 351 °F
Average value: 162 °C Grade Count:31
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..