Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 69.4 °C @Thickness 3.18 mm |
157 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 161J-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 69.4 °C @Thickness 3.18 mm |
157 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 161J-4-DD Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 69.4 °C | 157 °F | ASTM D648 |
Plaskolite Vivak PETG Sheet VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 69.4 °C @Thickness 1.57 mm |
157 °F @Thickness 0.0618 in |
Annealed; ASTM D648 |
PolyOne Novablend™ 4578 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 69.4 °C | 157 °F | ASTM D648 |
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 69.4 °C @Thickness 3.17 mm |
157 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
Teknor Apex APEX® RE 8003 Polyvinyl Chloride, Rigid Features: High Impact Resistance; Medium Gloss Processing Method: Extrusion Forms: Pellets Additional Information: Performance Characteristics: Yellow Card, Interior, Medium Gloss, Excellent FinishI.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 69.4 °C | 157 °F | ASTM D-648 |
Axiall 3121 Rigid PVC, Extrusion Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is sui.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 69.4 °C | 157 °F | Unannealed; ASTM D648 |
Multibase Multi-Flam™ 0106 PP Black Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |