Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 - 130 °C | 170 - 266 °F | Average value: 98.1 °C Grade Count:122 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 110 - 130 °C | 230 - 266 °F | ISO 75-A |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 39.0 - 130 °C | 102 - 266 °F | Average value: 92.7 °C Grade Count:13 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 55.0 - 130 °C | 131 - 266 °F | Average value: 81.1 °C Grade Count:24 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |