Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 215 - 235 °C | 419 - 455 °F | Average value: 218 °C Grade Count:13 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Deflection Temperature at 8.0 MPa | 215 °C | 419 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65 Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya.. |
|||
Deflection Temperature at 8.0 MPa | 215 °C | 419 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HTV-6H1 black 9205 PA6T/6I-GF60 Product description: Grivory HTV-6H1 black 9205 is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Deflection Temperature at 8.0 MPa | 215 °C | 419 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Deflection Temperature at 8.0 MPa | 215 °C | 419 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60 Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |