Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 135 °C
275 °F
Unannealed; ISO 75-2/C
PolyOne OnForce™ LFT PP-30LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-2
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength  (d
Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-2
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1, -2
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS.
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding-grade, 30% glass fibers, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
Lanxess Pocan® B 4239 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1,-2
Lanxess Durethan® BKV 30 N1 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
EMS-Grivory Grivory® BG-30 PA6-GF30
Product description: Grilon BG-30 is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 has the following important properties: High stiffnessGood balance between stre..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
EMS-Grivory Grivory® BG-30 S FA PA6-GF30
Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy ..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
EMS-Grivory Grivory® BG-30 S PA6-GF30
Product description: Grilon BG-30 S is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S has the following important properties: Excellent surface finishEasy flowin..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
EMS-Grivory Grivory® BG-30/2 PA6-GF30
Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSG-30 PA666-GF30
Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50
Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 5026 (BG-30 H) PA6-GF30
Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) bl..
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-2
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed
Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou..