Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® AG-30 PA66-GF30 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV XE 16101 (GVL-5H HP) PA*-GF50 Product description: Grivory XE 16101 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long special glass fibers. Grivory.. |
|||
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVL-5H nat PA*-GF50 Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na.. |
|||
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVX-7 H black 9915 PA*-GF70 Product description: Grivory GVX-7H black 9915 is a 70% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVX-7 H nat PA*-GF70 Product description: Grivory GVX-7H natural is a 70% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50 Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Deflection Temperature at 8.0 MPa | 220 °C | 428 °F | HDT/C; ISO 75-2 |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |