Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow) |
|||
Deflection Temperature at 8.0 MPa | 165 - 185 °C | 329 - 365 °F | ISO 75 C |
Vyncolit G885 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® AG-35 PA66-GF35 Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy .. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BG-35 PA6-GF35 Product description: Grilon BG-35 is a heat stabilized PA6 injection molding grade with 35% glass fibers. Grilon BG-35 has the following important properties: High stiffness Good surface finishEasy.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BG-35 S PA6-GF35 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BG-40 FC PA6-GF40 Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® G4V-5H nat PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-5H black PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50 Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-5H PA*-GF50 Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-50 PA666-GF50 Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSGZ-50 PA666-GF50 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 4134 black 9225 PA*-GF30 Product description: Grivory XE 4134 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVN-5H black 9915 PA*-GF50 Product description: Grivory GVN-5H is a 50 % glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | Unannealed; ISO 75-2/C |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-2/C |
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | HDT/C; ISO 75-2 |
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | HDT/C; ISO 75-2 |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | Unannealed; ISO 75-2/C |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
Lanxess Pocan® B 3235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-2 |
Hexion Bakelite™ PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability, good mechanical properties.Application areas: Insulating flanges, sealings, pulleys.Information p.. |
|||
Deflection Temperature at 8.0 MPa | 165 °C | 329 °F | ISO 75-1/-2 |
Lanxess Pocan® B 3235 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, improved flowability |