Polymer Property : Deflection Temperature at 8.0 MPa = 155 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 155 - 170 °C
311 - 338 °F
ISO 75 C
Vyncolit X658 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by ..
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30
Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi..
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30
Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSG-30/4 PA666-GF30
Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo..
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30
Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30
Product description: Grivory XE 4027 black 9916 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semicrystalline, partially aromatic copolyam..
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30
Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamid..
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30
Product description: Grivory HT1V-3 FWA black 9225 is a 30 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30
Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation ..
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30
Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl..
Deflection Temperature at 8.0 MPa 155 °C
311 °F
ISO 75-2
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m..