Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 125 - 150 °C
257 - 302 °F
ISO 75-C
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Deflection Temperature at 8.0 MPa 125 - 150 °C
257 - 302 °F
ISO 75-C
Raschig Group RALUPOL® 802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up..
Deflection Temperature at 8.0 MPa 125 - 150 °C
257 - 302 °F
ISO 75-C
Raschig Group RALUPOL® 804 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-2
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-2
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof  (discontinued **
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-2
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed  (disc
Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
Lanxess Durethan® AKV 30 HR H2.0 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
Lanxess Durethan® DP BKV 240 H2.0 901510 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers reinforced, elastomer-modified, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50
Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30
Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® BG-25 S PA6-GF25
Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-3 X ESD black PA12-GF30
Grilamid LV-3 X ESD black is an antistatic Polyamide 12 for injection molding with 30% glass fiber reinforcement. Main attributes are: antistatic with resistivity < 106 Ohmgood fuel and zinc chlorid..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-50H FWA black 9225 PA12-GF50
Product description: Grilamid LV-50H FWA black 9225 is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50
Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-5H PA12-GF50
Product description: Grilamid LV-5H is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 3915 PA12-GF50
Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® XE 4174 black 9992 PA1010-GF30
Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
EMS-Grivory Grivory® LC-3H black PA12-CF30
Product description: Grilamid LC-3H BLACK is a Polyamide 12 injection molding product reinforced with 30 % carbon fibers. The product is inherently black and is only available in this color.Main Att..
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-2
Hexion Bakelite™ PF 83 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets  (discontinued **)
Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Switch covers, rolls, handle casings..