Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 775 °C @Thickness 0.800 mm |
1430 °F @Thickness 0.0315 in |
Glow Wire Ignition Temperature; IEC 695-2-13 |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Glow Wire Test | 775 °C @Thickness 0.750 mm |
1430 °F @Thickness 0.0295 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
Glow Wire Test | 775 °C @Thickness 1.50 mm |
1430 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**) Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural.. |
|||
Glow Wire Test | 775 °C @Thickness 0.400 mm |
1430 °F @Thickness 0.0157 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Glow Wire Test | 775 °C @Thickness 3.20 mm |
1430 °F @Thickness 0.126 in |
IEC 60695-2-13 |
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
Glow Wire Test | 775 °C @Diameter 0.400 mm |
1430 °F @Diameter 0.0157 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Diameter 0.750 mm |
1430 °F @Diameter 0.0295 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Latamid 66 H2 G/35-V0KB3 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica.. |
|||
Glow Wire Test | 775 °C @Thickness 1.00 mm |
1430 °F @Thickness 0.0394 in |
GWIT |
LATI Laticonther 83 CP/80 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Glow Wire Test | 775 °C @Thickness 0.800 mm |
1430 °F @Thickness 0.0315 in |
Glow Wire Flammability Index, IEC 60695-2-12 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Valox® V9500GW PET+PC (Europe-Africa-Middle East) Unfilled Flameretardant PET/PC blend for GWIT.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Glow Wire Test | 775 °C @Thickness 1.50 mm |
1430 °F @Thickness 0.0591 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
DAM; IEC 60695-2-1/3 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
Glow Wire Test | 775 °C @Thickness 0.800 mm |
1430 °F @Thickness 0.0315 in |
ALL, Glow-Wire Ignition; IEC 60695-2-13 |
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecomid® NB40 NL FY70 PA6, flame retardant - halogen free (RoHS compliant), natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 1.50 mm |
1430 °F @Thickness 0.0591 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecomid® NB40 NL FA50 PA6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural Information provided by Eurotec® |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
DAM; Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret.. |
|||
Glow Wire Test | 775 °C @Thickness 0.750 mm |
1430 °F @Thickness 0.0295 in |
GWIT; IEC 60695-2-13 |
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Glow Wire Test | 775 °C @Thickness 2.00 mm |
1430 °F @Thickness 0.0787 in |
GWIT |
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion .. |
|||
Glow Wire Test | 775 °C @Thickness 3.00 mm |
1430 °F @Thickness 0.118 in |
IEC 60695-2-12 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |