Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 675 °C @Thickness 3.20 mm |
1250 °F @Thickness 0.126 in |
Glow Wire Ignition Temperature; IEC 695-2-13 |
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It .. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
DAM; IEC 60695-2-12 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 675 °C @Thickness 0.710 mm |
1250 °F @Thickness 0.0280 in |
DAM; IEC 60695-2-12 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glow Wire Test | 675 °C @Thickness 3.00 mm |
1250 °F @Thickness 0.118 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
Mitsubishi Xantar® C CM 206 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 675 °C @Thickness 0.750 mm |
1250 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Glow Wire Test | 675 °C @Thickness 0.750 mm |
1250 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Glow Wire Test | 675 °C @Thickness 3.00 mm |
1250 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Glow Wire Test | 675 °C @Thickness 3.00 mm |
1250 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Glow Wire Test | 675 °C @Thickness 0.750 mm |
1250 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Glow Wire Test | 675 °C @Thickness 0.750 mm |
1250 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Glow Wire Test | 675 °C @Thickness 3.00 mm |
1250 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Glow Wire Test | 675 °C @Thickness 0.810 mm |
1250 °F @Thickness 0.0319 in |
DAM; Ignition Temp; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
Glow Wire Test | 675 °C @Thickness 3.00 mm |
1250 °F @Thickness 0.118 in |
DAM; Ignition Temp; IEC 60695-2-13 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
Glow Wire Test | 675 °C @Thickness 3.00 mm |
1250 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
Glow Wire Test | 675 °C @Thickness 0.750 mm |
1250 °F @Thickness 0.0295 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Glow Wire Test | 675 °C @Thickness 3.00 mm |
1250 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Glow Wire Test | 675 °C @Thickness 0.850 mm |
1250 °F @Thickness 0.0335 in |
IEC 60695-2-12 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |
|||
Glow Wire Test | 675 °C @Thickness 0.850 mm |
1250 °F @Thickness 0.0335 in |
IEC 60695-2-12 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Sorona® 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature conditions... |
|||
Glow Wire Test | 675 °C @Thickness 3.00 mm |
1250 °F @Thickness 0.118 in |
IEC 60695-2-12 |
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Sorona® 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature conditions... |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a broad.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a broad.. |
|||
Glow Wire Test | 675 °C @Thickness 1.50 mm |
1250 °F @Thickness 0.0591 in |
Ignition; IEC 60695-2-13 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |