Polymer Property : Brittleness Temperature = 10.4 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable WJJC31L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D746-98
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D746
Teknor Apex APEX® 280-NL Polyvinyl Chloride, Flexible
Notes: 75°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D746
Teknor Apex APEX® 3302-90 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by..
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D746
Teknor Apex APEX® 3310-90 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D746
Teknor Apex APEX® 60001 Polyvinyl Chloride, Flexible
Notes: 75°C Insulation; RoHS Compliant Features: Flame Retardant Uses: Communication Wire InsulationAgency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; UL 13; UL 1..
Brittleness Temperature -12.0 °C
10.4 °F
Sylvin Technologies 6046 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Axiall 1063-119i Coax & Telecom Flexible PVC
Highly flame retardant CMR jacket for use over HDPE inners in 20-22 mil wall applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Axiall 22460 Coax & Telecom Flexible PVC
Non-lead stabilized, 75C rated PVC riser jacket over HDPE. Recommended minimum jacket thickness of 22 mils.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Axiall 36631 Coax & Telecom Flexible PVC
Semi-rigid, 80°C rated riser insulation compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Axiall 898 Wire & Cable Flexible PVC
Non-lead stabilized, flame retardant, non-migratory, 105°C insulation compound recommended for use in non-migratory applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo..
Brittleness Temperature -12.0 °C
10.4 °F
AlphaGary GW 2450-VW1 03 LCF Flame Retardant Polyvinyl Chloride
105°C rated insulation compound
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Axiall 2192 Wire & Cable Flexible PVC
Non-lead stabilized SJTO, SJTOO oil resistant flexible cord jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo..
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D746
Teknor Apex APEX® 1013 Polyvinyl Chloride, Semi-Rigid
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded ..
Brittleness Temperature -12.0 °C
10.4 °F
ASTM D-746
Axiall 4590 Flexible PVC
10 mil automotive thin wall insulation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -12.0 °C
10.4 °F
Cold Flex; ISO 458/2
Fainplast Compounds PM 9030 Flexible PVC, Lead Free
Various profiles