Polymer Property : Brittleness Temperature = -91.3 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -68.5 °C
-91.3 °F
Thickness = 1.90mm Conditioned for 40hrs at 23C at 50% RH; ASTM D746
PolyOne Versollan™ OM 1255NX-1 Thermoplastic Elastomer (TPE)
Versollan™ OM 1255NX-1 is a high performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Improved Grip with Matte, Rubbery Finish..
Brittleness Temperature -68.5 °C
-91.3 °F
Thickness = 1.90mm Conditioned for 40hrs at 23C at 50% RH; ASTM D746
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE)
Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi..