Thermal Properties Metric English Comments
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible 90250 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature <= -48.0 °C
<= -54.4 °F
TPE-0089 (ASTM D 746)
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber  (discontinued **)
A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Chevron Phillips KN 226B LDPE Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Chevron Phillips 1006 LDPE Injection Molding Resin  (discontinued **)
Resin Type: homopolymerCharacteristics: excellent flexibility, excellent flow, good warping resistance, moderate mold release, moderate ESCRApplications: large housewares, tamper evident snap-on cap..
Brittleness Temperature -48.0 °C
-54.4 °F
Sylvin Technologies 6404-78 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Teknor Apex APEX® 3201-55 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Teknor Apex APEX® 3301-55 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Teknor Apex APEX® 3311-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Teknor Apex Flexalloy® 9602-72FR Polyvinyl Chloride, Elastomer
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW;..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Teknor Apex APEX® 90-U656F1-72 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Brittleness Temperature <= -48.0 °C
<= -54.4 °F
ASTM D746
Teknor Apex Telcar® TL-1654B Thermoplastic Elastomer
Notes: Non-halogenated Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstr..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware..
Brittleness Temperature -48.0 °C
-54.4 °F
ISO 974
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Colorite Polymers 8588 Non-Phthalate 88 Series Vinyl Compound
Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo..
Brittleness Temperature -48.0 °C
-54.4 °F
Colorite Polymers Self Frosting™ 6011SF Vinyl Compound
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D-746
Axiall EX1264 Moldings & Extrusions Flexible PVC
General purpose extrusion compound designed for water stop applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer
Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D-746
Axiall 35061 Coax & Telecom Flexible PVC
CMR jacket over PVC or flame retardant PE insulation with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D-746
Axiall 37740 Wire & Cable Flexible PVC
90°C rated compound designed for use as an inner and outer jacket in Teck 90 cables.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -48.0 °C
-54.4 °F
AlphaGary PVC GSX 05-309 A2 UV Polyvinyl Chloride Thermoplastic
Lead free flexible compound
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Colorite Polymers 6000 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Teknor Apex APEX® 3050-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Brittleness Temperature -48.0 °C
-54.4 °F
Colorite Polymers 6011 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
Brittleness Temperature -48.0 °C
-54.4 °F
Colorite Polymers 6012 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable JG552NP Polyvinyl Chloride Alloy (PVC Alloy)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D746
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer
Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -48.0 °C
-54.4 °F
AlphaGary GW 2326 A VW1 LCF Flame Retardant Polyvinyl Chloride
90°C rated low temperature jacket compound.
Brittleness Temperature -48.0 °C
-54.4 °F
ASTM D-746
Axiall 38511 Wire & Cable Flexible PVC
Tray cable jacket with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Copyright © lookpolymers.com All Rights Reserved