Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brittleness Temperature = -54.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -47.8 °C
-54.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R108BM Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -47.8 °C
-54.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R130AE White 41 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -47.8 °C
-54.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R277AM Polyvinyl Chloride + NBR (PVC+NBR)
Information provided by PolyOne
Brittleness Temperature -47.8 °C
-54.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R5257A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Copyright © lookpolymers.com All Rights Reserved