Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable 8800FR Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W1200 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W84592L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D746 |
Teknor Apex Fireguard® 910-LBF Polyvinyl Chloride, Flexible RoHS Compliant Features: Bromine Free; Flame Retardant; Low Smoke Emission Uses: Insulation; Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC.. |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D746 |
Teknor Apex APEX® 4020 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D746 |
Teknor Apex APEX® 65012 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D746 |
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer Zythane™ 4065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | |
AlphaGary Smokeguard™ LS III 1041 B Low Smoke Polyvinyl Chloride Azoxymethane Free Low Cost Fiber Optic Jacket/Buffer Compound. Application example includes Optical Cables |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D-746 |
Axiall 1275 Plenum Flexible PVC Plenum-grade optical fiber jacket. UL QMTM2 recognized component for plenum cable compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D-746 |
Axiall 15640 Wire & Cable Flexible PVC Semi-rigid UL style #1061.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D-746 |
Axiall 15644 Wire & Cable Flexible PVC Semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | |
AlphaGary Smokeguard™ LS III 1041 Low Smoke Polyvinyl Chloride Azoxymethane Free Low Cost Fiber Optic Jacket/Buffer Compound. Application example includes Optical Cables |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | |
AlphaGary Smokeguard™ LS III 1042 B Low Smoke Polyvinyl Chloride Azoxymethane Free Low Cost Category Cable Jacket/Insulation |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | |
AlphaGary Smokeguard™ LS III 1056 Low Smoke Polyvinyl Chloride 75°C Plenum Jacket |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | |
AlphaGary Smokeguard™ LS III 1057 Low Smoke Polyvinyl Chloride 75°C Plenum Jacket |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | |
AlphaGary Smokeguard™ LS III 1042 Low Smoke Polyvinyl Chloride Azoxymethane Free Low Cost Category Cable Jacket/Insulation |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D-746 |
Axiall 01540 Plenum Flexible PVC CAT 5 rated plenum jacket. UL QMTM2 Plenum Cable Compound Component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -5.00 °C | 23.0 °F | ASTM D746-79 |
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(discon Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |