Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -32.2 °C | -26.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3772 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -32.2 °C | -26.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R252AE Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Brittleness Temperature | -32.2 °C | -26.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R252BE Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Brittleness Temperature | -32.2 °C | -26.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R3035E Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -32.2 °C | -26.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R313AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -32.2 °C | -26.0 °F | ASTM D746 |
Teknor Apex APEX® 3211-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |