Polymer Property : Brittleness Temperature = -30.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -30.6 °C
-23.1 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible D9501 NATURAL Polyvinyl Chloride, Flexible (PVC, Flexible)
A highly filled PVC Compound for extrusion applications.Information provided by PolyOne
Brittleness Temperature -30.6 °C
-23.1 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R 960A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -30.6 °C
-23.1 °F
TR-10
DuPont Performance Polymers VTR GLT Peroxide Cured Fluoroelastomer (FKM) Formulation
FormulationViton® VTR-8500