Polymer Property : Brittleness Temperature = -134 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP390-01 Narrow Molecular Weight Copolymer
DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0..
Brittleness Temperature -92.0 °C
-134 °F
ASTM D746
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..