Thermal Properties | Metric | English | Comments |
---|---|---|---|
Working Point | 960 °C | 1760 °F | Viscosity 10<sup>4</sup> dPa s; ISO 7884-2 |
Schott Glass 8100 Lead Glass Lead glass (33.5% PbO), electrically highly insulating, highly x-ray-absorbing TV tubesInformation provided by SCHOTT AG. |