Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Mechanical without Impact = 95.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 1.50 mm
203 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 1.70 mm
203 °F

@Thickness 0.0669 in
UL 746
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 1.50 mm
203 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 1.70 mm
203 °F

@Thickness 0.0669 in
UL 746
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness >=1.50 mm
203 °F

@Thickness >=0.0591 in
LG Chemical LUCEL N127LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Mechanical without Impact 95.0 °C

@Thickness >=1.50 mm
203 °F

@Thickness >=0.0591 in
LG Chemical LUCEL N145LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 0.810 mm
203 °F

@Thickness 0.0319 in
UL 746
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 1.50 mm
203 °F

@Thickness 0.0590 in
UL 746
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 0.810 mm
203 °F

@Thickness 0.0319 in
UL 746
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 1.50 mm
203 °F

@Thickness 0.0590 in
UL 746
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 0.750 mm
203 °F

@Thickness 0.0295 in
DAM; UL 746B
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6  (Unverified Data**)
Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 0.750 mm
203 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 1.50 mm
203 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 1.50 mm
203 °F

@Thickness 0.0591 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 0.750 mm
203 °F

@Thickness 0.0295 in
UL 746B
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM
Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri..
UL RTI, Mechanical without Impact 95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746B
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM
Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri..