Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 100 °C @Thickness >=0.710 mm |
212 °F @Thickness >=0.0280 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness >=1.50 mm |
212 °F @Thickness >=0.0591 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness >=3.00 mm |
212 °F @Thickness >=0.118 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness >=3.00 mm |
212 °F @Thickness >=0.118 in |
|
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness >=3.00 mm |
212 °F @Thickness >=0.118 in |
|
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness >=0.750 mm |
212 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness >=0.750 mm |
212 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness 1.50 mm |
212 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**) Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene.. |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness 0.750 mm |
212 °F @Thickness 0.0295 in |
|
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness 0.400 mm |
212 °F @Thickness 0.0157 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness 0.750 mm |
212 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness 1.50 mm |
212 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness 0.750 mm |
212 °F @Thickness 0.0295 in |
UL 746B |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness 0.400 mm |
212 °F @Thickness 0.0157 in |
UL 746B |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
UL RTI, Mechanical without Impact | 100 °C @Thickness 1.50 mm |
212 °F @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |