Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 100 °C

@Thickness 0.750 mm
212 °F

@Thickness 0.0295 in
UL 746
PolyOne Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)
These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended..
UL RTI, Mechanical with Impact 100 °C

@Thickness 0.750 mm
212 °F

@Thickness 0.0295 in
UL 746
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66)
Information provided by PolyOne
UL RTI, Mechanical with Impact 100 °C

@Thickness >=0.750 mm
212 °F

@Thickness >=0.0295 in
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
UL RTI, Mechanical with Impact 100 °C

@Thickness >=0.750 mm
212 °F

@Thickness >=0.0295 in
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant
Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che..
UL RTI, Mechanical with Impact 100 °C

@Thickness >=1.50 mm
212 °F

@Thickness >=0.0591 in
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
UL RTI, Mechanical with Impact 100 °C

@Thickness >=3.00 mm
212 °F

@Thickness >=0.118 in
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
UL RTI, Mechanical with Impact 100 °C

@Thickness >=1.50 mm
212 °F

@Thickness >=0.0591 in
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
UL RTI, Mechanical with Impact 100 °C

@Thickness >=3.00 mm
212 °F

@Thickness >=0.118 in
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
UL RTI, Mechanical with Impact 100 °C

@Thickness 1.50 mm
212 °F

@Thickness 0.0591 in
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi..
UL RTI, Mechanical with Impact 100 °C

@Thickness 3.00 mm
212 °F

@Thickness 0.118 in
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi..
UL RTI, Mechanical with Impact 100 °C

@Thickness 0.710 mm
212 °F

@Thickness 0.0280 in
UL746B
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Mechanical with Impact 100 °C

@Thickness 0.710 mm
212 °F

@Thickness 0.0280 in
UL746B
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Mechanical with Impact 100 °C

@Thickness 3.00 mm
212 °F

@Thickness 0.118 in
UL 746
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
UL RTI, Mechanical with Impact 100 °C

@Thickness 3.00 mm
212 °F

@Thickness 0.118 in
UL 746
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
UL RTI, Mechanical with Impact 100 °C

@Thickness 3.00 mm
212 °F

@Thickness 0.118 in
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded
AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
UL RTI, Mechanical with Impact 100 °C

@Thickness 0.750 mm
212 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
UL RTI, Mechanical with Impact 100 °C

@Thickness 1.50 mm
212 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
UL RTI, Mechanical with Impact 100 °C

@Thickness 1.50 mm
212 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
UL RTI, Mechanical with Impact 100 °C

@Thickness 0.750 mm
212 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded
Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas..
UL RTI, Mechanical with Impact 100 °C

@Thickness 1.50 mm
212 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded
Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas..