Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 125 °C @Thickness 0.800 mm |
257 °F @Thickness 0.0315 in |
UL 746 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Electrical | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Electrical | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
UL RTI, Electrical | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
UL RTI, Electrical | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
UL RTI, Electrical | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
UL RTI, Electrical | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
UL RTI, Electrical | 125 °C @Thickness 0.800 mm |
257 °F @Thickness 0.0315 in |
UL 746 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
UL RTI, Electrical | 125 °C @Thickness >=1.50 mm |
257 °F @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Electrical | 125 °C @Thickness >=1.50 mm |
257 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL GP3156F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided .. |
|||
UL RTI, Electrical | 125 °C @Thickness >=3.00 mm |
257 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Electrical | 125 °C @Thickness >=3.00 mm |
257 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0590 in |
UL 746 |
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex.. |
|||
UL RTI, Electrical | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
|
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
UL RTI, Electrical | 125 °C @Thickness 0.800 mm |
257 °F @Thickness 0.0315 in |
|
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
UL RTI, Electrical | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
UL RTI, Electrical | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
UL RTI, Electrical | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
UL RTI, Electrical | 125 °C @Thickness 0.810 mm |
257 °F @Thickness 0.0319 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
UL RTI, Electrical | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |