Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 700 °C @Thickness 2.00 mm |
1290 °F @Thickness 0.0787 in |
Flammability Index; IEC 60695-2-12 |
PolyOne OnFlex™ S EH 80A-3S7005 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Glow Wire Test | 700 °C @Thickness 2.00 mm |
1290 °F @Thickness 0.0787 in |
CEI 695-2-1/2 |
Radici Raditer® B RV 100 Polybutylene Terephthalate with 10% Glass fiber Raditer® B RV 100 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Glow Wire Test | 700 °C @Thickness 2.00 mm |
1290 °F @Thickness 0.0787 in |
CEI 695-2-1/2 |
Radici Raditer® B RV 200 Polybutylene Terephthalate with 20% Glass fiber Raditer® B RV 200 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Glow Wire Test | 700 °C | 1290 °F | GWFI; IEC 60695-2-12 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Glow Wire Test | 700 °C @Thickness 2.00 mm |
1290 °F @Thickness 0.0787 in |
GWFI; IEC 60695-2-12 |
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Glow Wire Test | 700 °C @Thickness 2.00 mm |
1290 °F @Thickness 0.0787 in |
GWFI; IEC 60695-2-12 |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Glow Wire Test | 700 °C @Thickness 2.00 mm |
1290 °F @Thickness 0.0787 in |
GWFI; IEC 60695-2-12 |
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
Glow Wire Test | 700 °C @Thickness 1.60 mm |
1290 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding specially stabilized to improve its resistance automotive cooling liquids.Available in: Europe and Latin Americ.. |
|||
Glow Wire Test | 700 °C @Thickness 1.60 mm |
1290 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, DRY Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: EuropeProduct Applications: TECHNYL A 218W V3.. |
|||
Glow Wire Test | 700 °C | 1290 °F | ISO 60695-2-12 |
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Glow Wire Test | 700 °C | 1290 °F | ISO 60695-2-12 |
Solvay TECHNYL® A 222 Black 1N PA66, DRY Description: Unreinforced polyamide PA66, medium viscosity, heat stabilized, for injection molding, fast crystallization, for short cycles .Available in: EuropeProduct Applications: TECHNYL A 222 of.. |
|||
Glow Wire Test | 700 °C @Thickness 1.60 mm |
1290 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Asia Pacific) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Europe-Africa-Middle East) NORYL* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade, targeted for flat panel TV enclosures. It has a Vicat B/120 temperature of 96 degC and UL-94 V0 @ 1.5mm .. |
|||
Glow Wire Test | 700 °C @Thickness 1.60 mm |
1290 °F @Thickness 0.0630 in |
IEC-60695-2-12 |
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu.. |
|||
Glow Wire Test | 700 °C | 1290 °F | G.W.I.T.; IEC 60695 |
Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant Flame retardant ABS for injection molding applications.Information provided by Polyram. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Glow Wire Test | 700 °C | 1290 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |